Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
News
Easy Fashion Metal Products Co., Ltd.
Home ProductsVacuum Sintering Furnace

Large High Temperature Sintering Furnace  , Superalloy Metal Sintering Machine

China Easy Fashion Metal Products Co., Ltd. certification
China Easy Fashion Metal Products Co., Ltd. certification
We purchased the 25kg Water atomization metal powder production fine from the EasyFashion industry, for metal powder production. The company have passed IS09001:2008 quality management system certification, the equipment is advanced in designing and obtaining relevant patents.

—— Toma Group

In our production, we achieved very good results. From the start of sintering training of qualified use up to now, the humanized mode, easy operation, good after-sales tracking service, stable operation and no maintenance record, all these impressed us greatly. So, right here, all our engineers agreed to recommend the equipment to other users.

—— Mr. Mohammed

I'm Online Chat Now

Large High Temperature Sintering Furnace  , Superalloy Metal Sintering Machine

Large High Temperature Sintering Furnace  , Superalloy Metal Sintering Machine
Large High Temperature Sintering Furnace  , Superalloy Metal Sintering Machine

Large Image :  Large High Temperature Sintering Furnace  , Superalloy Metal Sintering Machine

Product Details:
Place of Origin: China
Brand Name: EasyFashion Industry
Certification: CE Certificate
Model Number: GN5518A
Payment & Shipping Terms:
Minimum Order Quantity: 1 set
Packaging Details: Standard packed by wooden cases and container.
Delivery Time: 120 days
Supply Ability: 10 set per year
Detailed Product Description
Ultimate Vacuum: ≤2Pa, Tested In Cold And Clean Chamber Dimension Of Furnace: 4500×5400×3500 Mm
Dimension Of Usable Space: 500×500×1800 Mm Max. Load Weight: 1500 Kg
Wax Collecting Rate: ≥98﹪ Stand Area: ≈5200×6000 Mm
High Light:

zirconia sintering furnace

,

continuous sintering furnace

  • High Temperature Uniformity Vacuum Sintering And De-waxing Furnace For Superalloy

 

 Main Description

Integrated Vacuum Degreasing and Sintering Furnace integrate the functions of de-waxing, sintering, atmosphere controlling and cooling etc.

 

Technical specifications

Model

GN5518A GN3312A

Rated voltage

380 V 50 Hz, three-phase five-wire

Dimension of usable space

500×500×1800 mm 300×300×1200mm

Dimension of furnace

4500×5400×3500 mm 4500×4250×3500 mm

Max. load weight

1500 kg 500 kg

Weight of furnace

≈5500 kg ≈4000 kg

Stand area

≈5200×6000 mm ≈4500×4000mm

Power

340 kVA 200 kVA

Max. testing temperature

1600°C

Max. working temperature

≤1550°C

Temperature control method

3 zones

Ultimate vacuum

≤2Pa, tested in cold and clean chamber

 

Pumping speed

(in cold and clean chamber)

≤20 min., pumping from 1.13×105Pa to 5Pa

Com deviation

≤±0.2%

Temperature increasing rate (without loading)

15°C/min(≤1000℃);

10°C/min(≥1000℃)

Temperature uniformity

≤±7°C

(Ceramic ring)

Vacuum Leak rate

≤2Pa/h(24 hours average), tested in cold and clean chamber

Hc deviation

≤±0.3KA/M

Wax collecting rate

≥98﹪

Cooling speed

(without loading)

(cooling water ≤30°C)

From working temp. to 800°C, ≤ 3 h

From 800°C to opening door, ≤ 6 h

From working temp. to 800°C, ≤ 2 h

From 800°C to opening door, ≤ 5 h

 

 

 

 

 